摘 要:介绍煤棒制作的工艺和要求,即原料煤粉含水质量分数<8%,配制后原料含水质量分数<13%,沤化时间一般为24 h,烘干后煤棒含水质量分数<4%。以煤棒制气时,应适当提高入炉蒸汽压力和汽量,炉上温度一般控制在(280±20)℃,炉下温度一般控制在(300±20)℃,并应调整吹风百分比,增加下灰次数。采用煤棒制气,可充分利用碎煤、粉煤,吨氨成本下降140元,吨尿素成本下降90元以上,经济效益显著。
关键词:煤棒;制气;总结
Sum-Up of Use of Coal Rod for Gasification
Yao Liexia,Jing Wenge
(Shanxi Yongji Zhongnong Chemical Co.,Ltd. 044500)
Abstract:The process and requirements are given for the manufacture of coal rods,viz.,feed coal powder with a water content of <8% mass fraction,water content of feed afte....